Grade | Chemical composition at cast (% max.) | Delivery condition | Mechanical properties | ||||||
designation | C | N | Condition | Symbol | Re | Rm | % El min. | ||
N/mm2 | N/mm2 | A80 | A50 | Lo= 5.65 √So | |||||
Annealed | G | - | 270 - 350 | 38 | - | 40 | |||
Skin passed | LG | max. 210 | 270 - 350 | 38 | - | 40 | |||
K32 | 220 - 325 | 290 - 390 | 24 | - | 28 | ||||
- | - | - | - | - | - | ||||
St 4 | 0.08 (0.09) | - | Work | K40 | min. 350 | 390 - 490 | 6 | - | 14 |
hardened | - | - | - | - | - | - | |||
K50 | min. 460 | 490 - 590 | - | - | - | ||||
K60 | min. 560 | 590 - 690 | - | - | - |