8021| 27
|
cr12淬火硬度55度漏加工三個孔,,求助 |
| ||
| ||
點評
OSG的WH55-5D就能干了,,另外補充一點WH70-DRL和SH-DRL最高能干到70HRC
| ||
點評
直線度要求如何,?
| ||